Music: Bensound • http://www.warmtips.com/20060530.htm • Firing schedules (Bullseye) • First 3 firings • Segment 1 • 222°C/hr (400°F)→ 677°C (1250°F)30 min • Segment 2 • 333°C/hr (600°F) → 790°C (1454°F)10 min • Segment 3 • 999°C/hr (999°F)→ 482°C (900°F)60 min • Segment 4 • 83°C/hr (150°F)→ 371°C (700°F)End • Bubble Squeeze • Segment 1 • 150°C/hr ( 302°F )→ 600°C (1112°F)90 min • Segment 2 • 111°C/hr ( 200°F )→ 677°C (1250°F)90 min • Segment 3 • 333°C/hr ( 600°F ) → 804°C (1480°F)10 min • Segment 4 • 999°C/hr ( 999°F )→ 482°C (900°F)90 min • Segment 5 • 83°C/hr ( 150°F )→ 371°C (700°F)End • Slumping • Segment 1 • 150°C/hr (302°F) → 640°C (1184°F)20 min • Segment 2 • 999°C/hr (999°F)→ 482°C (900°F)90 min • Segment 3 • 56°C/hr (100°F)→ 371°C (700°F)End

#############################