I attempt to alloy copper and aluminum together while in a molten state. Interesting idea, but it doesn't go as planned. • The idea was to get swirls of different metals in the casting. Mixing the two together in 1 crucible would have made 1 homogeneous alloy, not produced swirl patterns. • I may do some experimenting with the same idea but using tin and zinc to make bronze/brass. It all depends on what the alloys of these metals will produce. If I can find one that doesn’t produce a weak and brittle alloy it might still work. • FYI the boiling temperature of aluminum is 4400F. • MERCH STORE!: • www.farmcraft101.com • Buy me a coffee- or a beer! • https://www.buymeacoffee.com/farmcraf... • Facebook: •   / farmcraft101   • Patreon: •   / farmcraft101  

#############################